A Chinese research team has developed a novel ultraviolet (UV)-converting polyolefin elastomer (POE) encapsulant for back-contact silicon solar modules, with the aim of improving their long-term reliability and mitigating UV-induced and potential-induced degradation (PID).

The researchers sought to overcome the limitations of conventional UV-converting encapsulants, in which physically blended additives can migrate through the polymer matrix, compromising electrical insulation and moisture-barrier properties. To address this issue, they designed a reactive additive capable of forming covalent bonds with the polymer network during module lamination.

“In this study, a reactive down-conversion POE encapsulation film was developed by incorporating the benzotriazole derivative BTBA, which contains polymerizable C=C groups,” the researchers explained. “The disappearance of the C=C absorption band after lamination, together with the subsequent migration and crosslinking results, supports the proposed chemical incorporation and covalent immobilization of BTBA within the POE network.”

The scientists synthesized two benzotriazole derivatives using previously reported procedures: 2-tert-butyl-4,7-bis[4-[(acryloyloxymethyl)methyl]phenyl]-2H-benzotriazole (BTBA), which served as the reactive additive, and 2-tert-butyl-4,7-bis[4-[(1-methylpropoxy)methyl]phenyl]-2H-benzotriazole (BTBM), which served as a physically blended reference additive.

They incorporated BTBA into the POE matrix at concentrations of 0.3 wt%, 0.6 wt%, and 0.9 wt%. They also fabricated reference films containing 0.6 wt% BTBM and baseline films containing neither UV-converting additive.

The team extruded the formulations into 0.45 mm-thick films and used them to encapsulate n-type monocrystalline back-contact solar cells in glass-glass mini-modules. The lamination process involved six minutes under vacuum followed by 10 minutes at 148 C.

The academics used infrared spectroscopy to investigate the curing behavior of BTBA, monitored additive migration at 150 C, and assessed the films’ physical properties and adhesion performance.


Source link

Disclaimer

We strive to uphold the highest ethical standards in all of our reporting and coverage. We TheMorningPulse.fyi want to be transparent with our readers about any potential conflicts of interest that may arise in our work. It's possible that some of the investors we feature may have connections to other businesses, including competitors or companies we write about. However, we want to assure our readers that this will not have any impact on the integrity or impartiality of our reporting. We are committed to delivering accurate, unbiased news and information to our audience, and we will continue to uphold our ethics and principles in all of our work. Thank you for your trust and support.